A series of welds were fabricated in mild (ASTM A36) steel. The first pass was the entire length of the plate and each subsequent pass was indented ∼25 mm. This allowed us to determine the change in hardness on a pass by pass basis by mapping the hardness over each weld pass.
MoonD. W., LambrakosS. G., WongR. J. and MetzbowerE. A.: Sci. Technol. Weld. Join., 2003, 8, (2), 95–101.
2.
MoonD. W., LambrakosS. G., WongR. J. and MetzbowerE. A.: Sci. Technol. Weld. Join., 2003, 8, (5), 334–339.
3.
MetzbowerE. A., MoonD. W., FengC. R., LambrakosS. G. and WongR. J.: in ‘Mathematical modelling of weld phenomena 7’, (ed. H. Cerjak et al.), 327–339; 2005, Cambridge, the University of Cambridge.
4.
MoonD. W., FengC. R.LambrakosS. G. and MetzbowerE.A.: in ‘Trends in welding research’ (ed. S. A. David et al.), 725–730, 2006, Metals Park, OH, ASM International.
5.
MoonD. W., FondaR. W. and SpanosG.: Weld. J., 2000, 79, 278s–285s.