Thin film measurements by energy dispersive x-ray analysis require appropriate standards. A method for preparing such standards by deposition of thin films and direct measurements of their thickness with a scanning electron microscope is described. These standards have been used to measure thickness of corrosion layers to within ±8.0 nm accuracy.
BirksL. S., Chemical Analysis (Wiley-Interscience, New York, 1971).
2.
AndersonC. R., Ed. Microprobe Analysis (Wiley-Interscience, New York, 1973).
3.
PowellC. F.OxleyJ. H., and BlockerJ. M.Jr., Vapor Deposition (Wiley, New York, 1966).
4.
AbbottW. H.WilliamsD. N.DettoreJ. F.GainesG. B.KisselJ. W.GlaeserW. A., and OgdenH. R., First Annual Report (Battelle Memorial Institute, Columbus, 1966).
5.
CampbellW. E., and ThomasU. V., in Proceedings of the Holm Seminar on Electric Contracts. (IIT Research Institute, Chicago, 1968), pp. 233ff.