Abstract
The mode-I and mode-II interlaminar fracture properties of high modulus pitch-based carbon fiber reinforced polymers (CFRPs) (fiber: K13C; resin: EX-1515 cyanate ester) modified with 20–30 nm β-SiC nanoparticles or multiwalled-carbon nanotubes (MWCNTs) were investigated. Different volume fractions of both the β-SiC nanoparticles (1, 2, 5, and 10 vol%) and MWCNTs (1, 3, 5, and 7 vol%) were tested. The values of the mode-I and mode-II interlaminar fracture toughness of the CFRPs containing the lowest volume fractions of these nanostructures were larger compared with the unfilled composite but decreased with increasing the volume fraction of the inclusions. No differences in mechanical properties were observed among the different nanostructure types.
Get full access to this article
View all access options for this article.
References
Supplementary Material
Please find the following supplemental material available below.
For Open Access articles published under a Creative Commons License, all supplemental material carries the same license as the article it is associated with.
For non-Open Access articles published, all supplemental material carries a non-exclusive license, and permission requests for re-use of supplemental material or any part of supplemental material shall be sent directly to the copyright owner as specified in the copyright notice associated with the article.