Abstract
Effect of solution treatment on the micropore and mechanical properties is investigated for the DD6 superalloy. The results show that solution treatment has positive and negative effects on the DD6 superalloy, which can weaken the segregation significantly. After solution treatment, the segregation ratio of the major alloying elements tends to 1. However, the amount of micropores increases with increasing solutionising time and can reach 0.46%, which is one order of magnitude higher than that of the as-cast superalloy. The hardness increases slightly, especially for the superalloy solutionised at 1310°C with a 5% increase in hardness compared to the as-cast superalloy. Hardness, tensile and stress rupture properties of the DD6 superalloy can reach the best after solution treatment at 1310°C and 4 h.