The degradation of pyromellitic acid diester (PMDE) was studied by transmission Fourier transform IR spectroscopy (FT-IR). Reaction temperatures were varied from room temperature to 280°C, and the effect of temperature upon the observed vibrational modes of PMDE was monitored and analyzed. The formation of both a cyclic and a noncyclic anhydride was observed.