Abstract
A mesoporous ZSM-5 monolith several millimetres in size has been synthesized employing the template method and using a carbon aerogel with uniform mesopores. Measurement of the pore-size distribution using nitrogen adsorption showed a bimodal pore system of mesopores and micropores whose average pore widths were 8 nm and 0.51 nm, and whose volumes were 0.09 cm3/g and 0.34 cm3/g, respectively.
References
1.
Argauer
R.J.
Landolt
G.R.
(1972 ) US Pat. 3 702 886 .
2.
Gabelic
Z.
Derouane
E.G.
(1984 ) ACS Symp. Ser. 248 , Am. Chem. Soc. , Washington, DC .
3.
Hanzawa
Y.
Kaneko
K.
(1998 ) Adsorption 4 , 187 .
4.
Herrmann
C.
Haas
J.
Fetting
F.
(1987 ) Appl. Catal. 35 , 299 .
5.
Jacobsen
C.J.H.
Madsen
C.
Houzvicka
J.
Schmidt
I.
Carlsson
A.
(2000 ) J. Am. Chem. Soc. 122 , 7116 .
6.
Ogura
M.
Shinomiya
S.
Tateno
J.
Nara
Y.
Kikuchi
E.
Matsukata
M.
(2000 ) Chem. Lett. 882 .
7.
Pekala
R.W.
Alviso
C.T.
(1992 ) Mater. Res. Soc. Symp. Proc. 270 , 3 .
8.
Suzuki
T.
Okuhara
T.
(2001 ) Microporous Mesoporous Mater . 43 , 83 .
9.
Wu
E.L.
Lawton
S.L.
Olson
D.H.
Rohrman
A.C.
Jr.
Kokotailo
G.T.
(1979 ) J. Phys. Chem. 83 , 2777 .