During a programme of transition temperature tests on 6-ft wide plates, strain gauge records, showing the strain field in the plates during fracture, were obtained. This report gives a few typical records and an interpretation of what they mean in terms of the behaviour of the metal when fractured. A possible explanation of how the fracture is self-sustained is also included.
WellsA. A.PostD.‘Dynamic stress distribution surrounding a running crack: a photoelastic analysis’, Proc. Soc. exp. Stress Anal.195816 (No. 1), 69.
3.
RobertsonT. S.‘Experimental techniques developed in investigations into high-speed yield in brittle fracture’, Proc. Conf. Properties Materials at High Rates of Strain, Instn mech. Engrs, Lond. 1957, 22.