Oxide dispersion strengthened steels are new generation alloys that are usually processed by hot isostatic pressing (HIP). In this study, spark plasma sintering (SPS) was studied as an alternative consolidation technique. The influence of the processing parameters on the microstructure was quantified. The homogeneity of the SPSed materials was characterised by electron microprobe and microhardness. A combination of limited grain growth and minimised porosity can be achieved on semi-industrial compact. Excellent tensile properties were obtained compared to the literature.
de CarlanY, BechadeJ.-L, DubuissonP, SeranJ.-L, BillotP, BougaultA, CozzikaT, DoriotS, HamonD, HenryJ, RattiM, LochetN, NunesD, OlierP, LeblondT and MathonMH: ‘CEA developments of new ferritic ODS alloys for nuclear applications’, J. Nucl. Mater., 2009, 386–388, 430–432.
2.
KluehRL, GellesDS, JitsukawaS, KimuraA, OdetteGR and van der SchaafB: ‘Ferritic/martensitic steels – overview of recent results’, J. Nucl. Mater., 2002, 307–311, (Part 1), 455–465.
3.
SarojaS, DasguptaA, DivakarR, RajuS, MohandasE, VijayalakshmiM, Bhanu Sankara RaoK and RajBaldev: ‘Development and characterization of advanced 9Cr ferritic/martensitic steels for fission and fusion reactors’, J. Nucl. Mater., 2011, 409, 131–139.
4.
FabrègueD, PiallatJ, MaireE, JorandY, Massardier-JourdanV and BonnefontG: ‘Spark plasma sintering of pure iron nanopowders by simple route’, Powder Metall., 2012, 55, 76–79.
5.
GrosdidierT, JiG and LaunoisS: ‘Processing dense hetero-nanostructured metallic materials by spark plasma sintering’, Scr. Mater., 2007, 57, (6), 525–528.
6.
GuoWM, YangZG and ZhangGJ: ‘Comparison of ZrB2-SiC ceramics with Yb2O3 additive prepared by hot pressing and spark plasma sintering’, Int. J. Refract. Met. Hard Mater., 2011, 29, 452–455.
7.
Bernard-GrangerG, MonchalinN and GuizardC: ‘Comparisons of grain size-density trajectory during spark plasma sintering and hot-pressing of zirconia’, Mater. Lett., 2008, 62, 4555–4558.
8.
BouvardD: ‘Métallurgie des poudres’; 2001, Bouvard, Hermes Science Publications.
9.
ChoSA, de ArenasIB and ArenasFJ: ‘Porosity: microhardness correlation of sintered (Al(1−y)Cry)2O3 solid solutions’, J. Alloys Compd, 1999, 288, 211–216.
10.
BoulnatX, PerezM, FabrègueD, DouillardT, MathonM.-H and de CarlanY: ‘Microstructure evolution in nano-reinforced ferritic steel processed by mechanical alloying and spark plasma sintering’, Metall. Mater. Trans. A, 2014, 45A, 1485–1497.
11.
CahoonJR, BroughtonWH and KutzakAR: ‘The determination of yield strength from hardness measurements’, Metall. Trans., 1971, 2, (7), 1979–1983.
12.
BoulnatX, FabrègueD, PerezM, MathonM.-H and de CarlanY: ‘High-temperature tensile properties of nano-oxide dispersion strengthened ferritic steels produced by mechanical alloying and spark plasma sintering’, Metall. Mater. Trans. A, 2013, 44A, (6), 2461–2465.
13.
SunQX, ZhangT, WangXP, FangQF, HaoT and LiuCS: ‘Microstructure and mechanical properties of oxide dispersion strengthened ferritic steel prepared by a novel route’, J. Nucl. Mater., 2012, 424, 279–84.
14.
AugerMA, de CastroV, LegueyT, MuñozA and ParejaR: ‘Microstructure and mechanical behavior of ODS and non-ODS Fe–14Cr model alloys produced by spark plasma sintering’, J. Nucl. Mater., 2013, 436, 68–75.
15.
WangY, ChenaM, ZhouF and MaE: ‘High tensile ductility in a nanostructured metal’, Nature, 2002, 322, 1–22.
16.
SakasegawaH, ChaffronL, LegendreF, BrocqM, BoulangerL, PoissonnetS, de CarlanY, BechadeJ, CozzikaT and MalaplateJ: ‘Evaluation of threshold stress of the MA957 ODS ferritic alloy’, J. Nucl. Mater., 2009, 386–388, 511–514.
17.
MalaplateJ, MompiouF, BéchadeJ.-L, Van Den BergheT and RattiM: ‘Creep behavior of ODS materials: a study of dislocations/precipitates interactions’, J. Nucl. Mater., 2011, 417, 205–208.