Abstract
In this paper, post‐treatments, including dehydrogenation process and passivation process for electroless Ni–P coating, are discussed. Porosity test and potentiodynamic polarisation curves were used to evaluate the porosity and corrosion resistance of electroless Ni–P coatings. The results indicated that the ideal dehydrogenation heat treatment temperature is 180–200°C. The passivation process can further increase the corrosion resistance of electroless Ni–P coating. Both dehydrogenation process and passivation process are essential to obtain compact, corrosion resistant electroless Ni–P coating.
Get full access to this article
View all access options for this article.
References
1.
Macko
R
,
Mason
T
: Plat. Surf. Finish ., Mar. 2000 , 10 .
2.
Baudrand
D
: Plat. Surf. Finish ., Nov. 1999 , 44 .
3.
Tung
S
,
Devin
TM
: Proc. 202nd Electrochemical Society Meet., Sat Lake City, UT, USA, October 2002, Electrochemical Society, Abstract G1-25 .
4.
Yan
H
: ‘New techniques in electroless nickel and composite plating’ , 1 ; 2001 , Beijing , Industry of National Defense Press
5.
Brenner
A
,
Couch
EG
,
Williams
EK
: J. Res. NBS , 1950 , 44 , 109 .
6.
De Minjer
CH
,
Brenner
A
: Plating , 1957 , 44 , 1297 .
7.
Crobu
M
,
Scorciapino
A
,
Elsener
B
: Electrochim. Acta , 2008 , 53 , 3364 .
8.
Hosseini
MG
,
Abdolmaleki
M
,
Seyed Sadjadi
SA
: Surf. Sci ., 2009 , 25 , 382 .
9.
Zeng
A
,
Xiong
W
,
Xu
J
: Mater. Lett ., 2005 , 59 , 524 .
10.
Huang
Y
,
Shi
K
,
Liao
Z
,
Wang
Y
: Mater. Lett ., 2007 , 61 , 1742 .
11.
Pan
XF
,
Mu
GH
,
Shen
HG
,
Gu
MY
: Appl. Surf. Sci ., 2007 , 253 , 4119 .
12.
Liu
Y
,
Zhao
Q
: Appl. Surf. Sci ., 2004 , 228 , 57 .
13.
Balaraju
JN
,
Jahan
SM
,
Jain
A
,
Rajam
KS
: J. Alloys Compd , 2007 , 436 , 319 .
14.
Balarju
JN
,
Rajam
KS
: Surf. Coat. Technol ., 2005 , 195 , 154 .
15.
Hu
XG
,
Cai
WJ
,
Xu
YF
,
Wan
JC
,
Sun
XJ
: Surf. Sci ., 2009 , 25 . 361 .
16.
Zhang
H
,
Liu
RL
: Mater. Proc ., 2007 , 39 , 56 .
17.
Alirezaei
S
,
Monirvaghefi
SM
,
Salehi
M
,
Saatchi
A
: Wear , 2007 , 262 , 978 .
18.
Liu
YY
,
Yu
J
,
Huang
H
,
Xu
BH
,
L Liu
X
,
Gao
Y
,
Dong
XL
: Surf. Coat. Technol ., 2007 , 201 , 7246 .
19.
Abdel Aal
A
,
Zaki
ZI
,
Abdel Hamid
Z
: Mater. Sci. Eng. A , 2007 , A447 , 87 .
20.
Hao
L
,
Wei
J
,
Gan
FX
: Surf. Eng ., 2009 , 25 . 372 .
21.
Feng
QF
,
Shen
W
,
Lin
A
: Mater. Prot ., 2009 , 41 , 25 .
22.
Zheng
Z
,
Yu
X
,
Sun
Y
,
Xue
F
,
Ren
S
: J. Chn Soc. Corros. Prot ., 2006 , 26 , 221 .
23.
Wang
LL
,
Chen
HJ
,
Huang
WQ
,
Hao
L
: Surf. Eng ., 2009 , 25 , 376 .
24.
Hu
W
,
Xiang
Y
,
Liu
X
,
Liu
L
,
Ding
W
: J. Chn Soc. Corros. Prot ., 2001 , 21 , 340 .
25.
Ma
J
,
Hu
J
,
Yan
D
,
Gao
Q
: Hebei J. Indust. Sci. Technol ., 2008 , 25 , 82 .
26.
Jiang
XX
,
Shen
W
: ‘The fundamental and practice of electroless plating’ ; 2000 , Beijing , Defence Industry Press .
27.
Han
TL
,
Liu
JQ
,
Luo
WY
: Mater. Prot ., 2005 , 38 , 31 .