Abstract
Laser nitriding of Ti–6Al–4V alloy was performed at different laser scanning speed. The results show that higher nitride concentration and microhardness are formed in the coatings laser nitrided with lower scanning speed. Nevertheless, higher nitride concentration results in higher residual stress which induces cracks occurring in the coatings.
Get full access to this article
View all access options for this article.
References
1.
Xin
H
,
Watson
LM
,
Baker
TN
: Acta Mater ., 1998 , 46 , 1949 .
2.
Nwobu
AIP
,
Rawlings
RD
,
West
DRF
: Acta Mater. , 1999 , 47 , 631 .
3.
Man
HC
,
Cui
ZD
,
Yue
TM
,
Cheng
FT
: Mater. Sci. Eng. A , 2003 , A355 , 167 .
4.
Man
HC
,
Cui
ZD
,
Yang
XJ
: Appl. Surf. Sci. , 2002 , 199 , 293 .
5.
Yilbas
BS
,
Uslan
CK
,
Keles
O
,
Usta
IY
,
Ahsan
M
: Appl. Surf. Sci. , 2006 , 252 , 8557 .
6.
Santos
EC
,
Morita
M
,
Shiomi
M
,
Osakada
K
,
Takahashi
M
: Surf. Coat. Technol. , 2006 , 201 , 1635 .
7.
Mridha
S
,
Baker
TN
: Mater. Sci. Eng. A , 1994 , A188 , 229 .
8.
Kloosterman
AB
,
de Hosson
J-ThM
: Scr. Metall. Mater. , 1995 , 33 , 567 .
9.
Pérez
MG
,
Harlan
NR
,
Zapirain
F
,
Zubiri
F
: Surf. Coat. Technol. , 2006 , 200 , 5152 .
10.
Abboud
JH
,
Fidel
AF
,
Benyounis
KY
: Opt. Laser Technol. , 2008 , 40 , 405 .
11.
Yang
YL
,
Zhao
GJ
,
Zhang
D
,
Liu
CS
: Acta Metall. Sinica , 2006 , 19 , 151 .
12.
Holmberg
K
,
Laukkanen
A
,
Ronkainen
H
,
Wallin
K
,
Varjus
S
,
Koskinen
J
: Surf. Coat. Technol. , 2006 , 200 , 3810 .
13.
Appel
F
,
Christoph
U
,
Oehring
M
: Mater. Sci. Eng. A , 2002 , A329–331 , 780 .
14.
Liu
XY
,
Chu
PK
,
Ding
CX
: Mater. Sci. Eng. R , 2004 , R47 , 49