The self-sensing of damage and strain in carbon fiber polymer-matrix structural composites has been attained by DC electrical resistance measurement. This paper reviews the self-sensing behavior, in addition to addressing the electrical contact configurations and providing a model for relating the resistance to the damage.
References
1.
BurkeS. K., CouslandS. M., and ScalaC. M., Materials Forum, 18, (1994), 85.
2.
AchenbachJ. D., International J. Solids & Structures, 37, (2000), 13.
FoedingerR. C., ReaD. L., SirkisJ. S., BaldwinC. S., TrollJ. R., GrandeR., DavisC. S., and VanDiverT. L., Proceedings of SPIE – the International Society for Optical Engineering, Bellingham, WA, 3670, (1999), 289.
5.
WhiteS. R., Proceedings of SPIE – the International Society for Optical Engineering, Bellingham, WA, 2442, (1995), 337.
6.
WangX., and ChungD. D. L., Composite Interfaces, 5, (1998), 191.
7.
WangX., and ChungD. D. L., Polymer Composites, 18, (1997), 692.
8.
WangX., and ChungD. D. L., Carbon, 35, (1997), 706.
9.
WangX., FuX., and ChungD. D. L., J. Materials Research, 14, (1999), 790.
10.
WangX., and ChungD. D. L., J. Materials Research, 14, (1999), 4224.
11.
WangS., and ChungD. D. L., Polymer Composites, 21, (2000), 13.
12.
MeiZ., GuerreroV. H., KowalikD. P., and ChungD. D. L., Polymer Composites, 23, (2002), 425.
13.
WangS., and ChungD. D. L., Polymer Composites, 22, (2001), 42.
14.
MutoN., YanagidaH., NakatsujiT., SugitaM., OhtsukaY., and AraiY., Smart Material Structures, 1, (1992), 324.
15.
WangX., WangS., and ChungD. D. L., J. Materials Science, 34, (1999), 2703.
16.
WangS., and ChungD. D. L., Composite Interfaces, 9, (2002), 51.
17.
WangX., and ChungD. D. L., Composite Interfaces, 5, (1998), 191.
18.
WangS., and ChungD. D. L., Composites: Part B, 30, (1999), 591.
19.
WangS., and ChungD. D. L., Polymers & Polymer Composites, 9, (2001), 135.
20.
MutoN., YanagidaH., MiyayamaM., NakatsujiT., SugitaM., and OhtsukaY., J. Ceramic Society Japan, 100, (1992), 585.
SugitaM., YanagidaH., and MutoN., Smart Material Structures, 4, (1995), A52.
24.
KaddourA. S., Al-SalehiF. A. R., Al-HassaniS. T. S., and HintonM. J., Composite Science and Technology, 51, (1994), 377.
25.
CeyssonO., SalviaM., and VincentL., Scripta Materialia, 34, (1996), 1273.
26.
SchulteK., and BaronCh., Composite Science and Technology, 36, (1989), 63.
27.
SchulteK., J. Physique IV, Colloque C7, 3, (1993), 1629.
28.
AbryJ. C., BochardS., ChateauminoisA., SalviaM., and GiraudG., Composite Science and Technology, 59, (1999), 925.
29.
TedorokiA., KobayashiH., and MatuuraK., JSME International J. Series A – Solid Mechanics Strength of Materials, 38, (1995), 524.
30.
HayesS., BrooksD., LiuT., VickersS., and FernandoG. F., Proceedings of SPIE – the International Society for Optical Engineering, Bellingham, WA, 2718, (1996), 376.
31.
WangS., and ChungD. D. L., Composites: Part B, 30, (1999), 376.
32.
WangS., and ChungD. D. L., Composite Interfaces, 6, (1999), 497.
33.
WangS., and ChungD. D. L., J. Materials Science, 35, (2000), 91.
34.
WangS., and ChungD. D. L., International J. Adhesion and Adhesives, 21, (2001), 465.
35.
WangS., KowalikD. P., and ChungD. D. L., J. Adhesion, 78, (2002), 189.
36.
ParkJ. B., OkabeT., TakedaN., and CurtinW. A., Composites: Part A, 14, (2002), 267.
37.
XiaoJ., LiY., and FanW. X., Composite Science and Technology, 59, (1999), 1369.