In this paper, thermal treatments of Kevlar-29 fiber resulted in a significant enhancement of compressive strength and corresponding decrease in tensile strength. These changes result from a decreased linearity at the macroscopic level in the fiber. Statistically designed experiments indicate that treatment temperature is the most significant variable in the thermal processing, while treatment soak time also played a role in the shift of properties.
Get full access to this article
View all access options for this article.
References
1.
[1] Tanner D, Fitzgerald J A and Phillips B R1989Adv. Mater5151-151
2.
[2] Krause S J, Haddock T B, Vezie D L, Lenhert P G, Hwang P G, Price W F, Helminiak T E, O'Brien J F and Adams W W1988Polymer291354-1354
3.
[3] Fawaz S A, Palazotto A N and Wang C S1992Polymer33100-100
4.
[4] Newell J A, Edie D D and Fuller E L Jr1996J. Appl. Polym. Sci.60825-825
5.
[5] Newell J A and Edie D D1996Carbon34551-551
6.
[6] Liang Y, Quichen Z and Warner S B1994J. Polym. Sci.A 322207-2207
7.
[7] Kumar S and Helminiak T E1990SAMPE J.2651-51
8.
[8] Allen S R1987J. Mater Sci.22853-853
9.
[9] Ballauff1989Angew Chem. Adv. Mater28135-135
10.
[10] Kenner J and Witham E1983]. (Chem. Soc.103232-232
11.
[11] Sweeny W1992J. Polym. Sci.A 301111-1111
12.
[12] McGarry F J and Moalli J E1991Polymer321811-1811
13.
[13] Barton R, Lee K and Schultz J M1995J. Polym. Sci.A 331-1
14.
[14] Newell J A and Puzianowski A A1999High Perform. Polym.11197-197
15.
[15] Newell J A, Rogers D K, Edie D D and Fain C C1994Carbon32651-651