Abstract
Formation of nanosized mixed semiconductor PbxCd1 —xS in situ into PEO—polymer electrolyte matrix at room temperature is reported. The disperse phase was identified by X-ray diffraction analysis. Optical microscopy shows the increase in amorphicity with dispersal of semiconductor while scanning electron microscope/ transmission electron microscope affirmed the formation of nanoparticulates with various sizes. The size distribution was further supported by Ultraviolet/Visible absorption of the colloid. The detailed electrical characterizations show that the dispersed PbxCd1—xS introduced a small (≤13%) electronic conductivity into pure ion conducting PEO:NH4I polymer electrolyte matrix.