The toxicities of the airborne combustion products of 11 textiles and 6 upholstery materials at medium temperatures (500-700 °C) were examined ac cording to the standard DIN 53436 using rats as experimental animals. Also the chemical composition of the combustion products was determined. According to the results obtained there were some cases in which one or more individual com ponents (mainly HCN and CO) of the airborne combustion products could be shown to be the main cause of toxicity.
Get full access to this article
View all access options for this article.
References
1.
Harland, W.A. and Woolley, W.D., Fire Int. , 6, 66, p. 37 (1979).
2.
Birky, M.M., Fire Mater., 3 , 4, p. 211 (1979).
3.
Kimmerle, G. and Prager, F.K., J. Comb. Toxicol.7, p. 42 (1980).
4.
Herpol, C., Fire Mater., 1, 1, p. 29 (1976 ).
5.
Producing Thermal Decomposition Products from Materials in an Air Stream and Their Toxicological Testing: Part 1. Test Method 53436Deutsches Institut für Normung, Berlin (in German) (1981).
6.
Standard Method Test for Nitrogen Dioxide Content of the Atmosphere: Test Method D-1607-69American Society for Testing and Materials.Philadelphia (1970).
7.
Pohjola, V., Manninen, A. and Häsänen, E., "Development and Study of Determination of Gaseous Impurities in Air," Technical Research Centre of Finland, Chemical Laboratory, Report 23 (in Finnish (1979).
8.
Klimisch, H.-J. , et. al., J. Comb. Toxicol , 7, p. 243 (1980).
9.
Hyvarinen, A., et. al. in Clinical Laboratory Studies, ed. by Werner Söderström, Porvoo, p. 450 (in Finnish) (1972).
10.
Herpol, C.Minne, R. and Outryve, E. Van, Comb. Sci Technol.12, p. 217 (1976).
11.
Levin, B.C., et al., "An Acute Inhalation Toxicological Evaluation of Combustion Products from Fire Retarded and Non-Fire Retarded Flexible Polyurethane Foam and Polyester,"Natural Bureau of Standards, NBSIR 83—2791, p. 18, Washington (1983).
12.
National Institute for Occupational Safety and Health (NIOSH).Registry of Toxic Effects of Chemical SubstancesU.S. Department of Health and Human Serivces , p. 761 ( 1980).
13.
Woolley, W.D. , Br. Polym. J., 4, p. 27 (1972).
14.
Kallonen, R., von Wright, A. and Tikkanen, L., "Toxicity of Fire Effluents from Textiles at Thermal Degradation Temperature of 600 °C," Technical Research Centre of Finland, Fire Technology Laboratory, Research Note 297 (in Swedish (1984).