Styrene butadiene rubber formulations utilizing Egyptian Kaolin as a filler, were evaluated against a commercial imported Kaolin sample.
Get full access to this article
View all access options for this article.
References
1.
J.B. De Coste and V.Y. Walder.1955. "Weathering of PVC,"Ind. Eng. Chem., 47(2):314-322.
2.
J.C. Hendricks and E.L. White.1952. "National Lead; Weathering Characteristisc of Polyvinyl chloride Plastics, Wire and Wire Production," October 1952.
3.
S. Wertham.1949. Off. Dig. Federation and Varnish Production Clubs, 292, 311.
4.
G.D. Prfitt and K.S.W. Sin.1976. Characterization of Powder SurfaceLondon: Academic Press, 9:428-455.
5.
S.M. El-Sawy .1992. J. Pigment and Resin Technology, Vol. 8.
6.
ASTM Designation, D 15-66T, 1967.
7.
ASTM Designation, D 412-66T, 1957.
8.
Shvats, A.1957. Kouch Rezina, 7:31.
9.
E.M. Abdel-Bary , A.G. El-Shekeil, F.M. Helaly, S.A. Sarhan and H.H. Abdel-Razek.1992. J. Plastics, Rubber and Composites Processing and Applications , 17:99-107.
10.
ASTM Designation D 814-40T. 1944. Revised 1946.
11.
El-Shami, S.M. , I.Z. Selim, I.M. El-Anwar and M.H. El-Mallah.1992. J. Am. Oil Chem. Soc, 69:872.