An accelerated humidity test utilizing a combination of high temperature and high humidity has been used to determine the ability of urethane and polyacrylate elastomers to withstand humid environments. A wide variation was found in the hydrolytic stability of the materials tested, which would not have been dis closed by the usual short term low temperature humidity test. The degradation has also been found to occur at moderate humidities as well, although the quantitative relationships of degradation rate versus relative humidity level has not as yet been accurately defined.
Get full access to this article
View all access options for this article.
References
1.
F.H. Gahimer and F.W. Nieske, "Navy Investigates Reversion Phenomena of Two Elastomers", Insulation, August 1968, pp. 39-44.
2.
F. O'Brien, "The Control of Humidity by Saturated Salt Solutions", Journal of Scientific Instruments, 25, (1948), p. 73.
3.
Technical Bulletin No. 5, "Creating and Maintaining Humidities by Salt Solutions", Hygrodynamics, Inc.
4.
E.B. Millard , Physical Chemistry for Colleges , McGraw-Hill Book Co. (1941), p. 436.
5.
D.V. Rosato and R.T. Schwartz, Environmental Effects on Polymeric Materials, Vol. 1, (1968), Interscience Publishers, pp. 1167-77.
6.
International Critical Tables 1, McGraw-Hill Book Co., p. 68.