Brunet. P.C. , and Coles. B.C., Tanned Silks, Proc. R. Soc. London B 187, 133-170 (1974).
2.
Kato, H., Structural Analysis of Bombyx mori Silk Yams Treated with Tannic Acid-Antimony Potassium Tartrate. and Wild Silk Yarns, Int. J. Wild Silkmoth Silk1, 84-92 (1994).
3.
Kawahasa, Y. , Shioya. M., Kikutani , T., and Takaku. A.Analysis of Swelling Behavior of Silk Fibers by Small-Angle X-Ray Scattering, Sen'i Gakkaishi50, 199-207 (1994).
4.
Magoshi. J., and Nakamura. S.Glass Transition and Crystallization of Silk fibroin, J. Appl. Polym. Sci.19, 1013-1015 (1975 ).
5.
Nagura. M., Urushidani. M.Shinohara. H., and Ishihara. H., Molecular Motion in Degummed Silk Fiber and Poly(L-alanine) Fiber . Kobunshi Ronbunshu35, 81-86 (1978).