Hot greasy wool was compressed to the same final density by using different amounts of wool in a biaxial press to achieve different amounts of compression in the two directions. The compressed wool was then cooled under restraint outside the press to find compression conditions for optimum strength, durability, and long-term packing density of the resultant blocks.
Get full access to this article
View all access options for this article.
References
1.
JamesJ. F. P.RichardsonA. M., Wool-Bale Tie Tensions and Strengths, J. Textile Inst.60, T223 (1969).
2.
PearsonA. J. C.WarnerJ. J., The Compression of Wools to Very High Bulk Densities. J. Textile Inst.74, T233 (1983).
3.
PrestonJ. M.WoodG. F., Producing Wool Packages of Very High Density, J. Textile Inst.58, T175 (1967).
4.
StearnA. E., The Effect of Anisotrophy in the Randomness of Fibre Orientation on Fibre to Fibre Contacts, J. Textile Inst.62, T353 (1971).
5.
WallsG. W., Minimum Volume Pressing of Greasy Wool, Textile Res. J.58, 43–50 (1988).
6.
WallsG. W., Pressing a Range of Wools in Instrumented Minimum Volume Presses, Textile Res. J.58, 102–110 (1988).