The load-elongation values of individual filaments in a multifilament yarn were studied. The behavior of individual filaments in a bundle is not the same as that of filaments tested individually; therefore, the load-elongation diagram of a multifilament yarn has to be used to arrive at tenacity values of individual filaments in a yam. A technique for obtaining load-elongation values of individual filaments was developed using the breaking steps in a load-elongation diagram of a multifilament yam. Preliminary results are described.
Get full access to this article
View all access options for this article.
References
1.
Gerasimova, L.S., and Gordeeva , L.A., Determination of the Degree of Preorientation of Capron Yarn for Birefringence, Fibre Chem.10, 164-165 (1978).
2.
Morton, W.E., and Hearle, J.W.S., "Physical Properties of Textile Fibres," 2nd ed., Heinemann.London. 1975, p. 265.
3.
Serova, V.A. , and Yasnikov, L.A., Statistical Analysis of the Measured Quality Indices of Polyester Filament Yarn, Fibre Chem.8, 587-590 (1976).
4.
Stein, W., Detecting Altered Spinning Conditions on Preoriented Polyester Filament Yam , Int. Textile Bull. Spinning, no. 3, 259-276 (1981).
5.
Zharov, V.B. , and Aleksandriiskii , S.S., Properties of Undrawn Polyester Yarn in Terms of the Load Extension Diagram, Fibre Chem.11, 134-137 (1979).