An estimation of the extent of fiber-fiber bonding in polymer-treated wool fabrics is achieved by sectioning yarns after they have been carefully unroved. To avoid contamination from mounting aids, the yarns were placed between two rectangular pieces of polyethylene in the microtome. The number of fiber snippets that remain as clusters are counted with the assumption that a fiber-fiber bond will result in two or more fibers per group. It is shown that the technique can be used to distinguish between the amounts of polymer applied.
Get full access to this article
View all access options for this article.
References
1.
BairdK.FouldsR. A., Felting Shrinkage of Plain-Knitted Wool Fabrics: Its Dependence Upon Fabric Structure and Shrinkproofing Level, Textile Res. J. 38, 743–753 (1968).
2.
BateupB. O.CookJ. R.FeltmannH. D.FleischfresserB. W.Effect of Environment on Adhesion of Shrink-Resist Polymers on Wool, Textile lies. J. 46, 796–801 (1976).
3.
ChakravartiI. M.LahaR. G.RoyJ., “Handbook of Methods of Applied Statistics,”Volume 1, John Wiley & Sons, New York, 1967.
4.
KershawA.LewisJ., The Role of Polymer Treatments in the Shrinkproofing of Wool, Textile Month, April, 40–44 (1976).
5.
MakinsonK. R., “The Ways in Which Resins Prevent Felting,” Proc. Int. Wool Textile Res. Conf., Australia, 1955.
6.
MakinsonK. R., Mechanisms of Shrink-Proofing with Silicone Resins, Textile Res. J. 45, 217–219 (1975).
7.
ShawT., The Felting of Wool: Its Uses and Prevention, Textiles5, No. 1, 2–7 (1976).
8.
StockC. R.SalleyD. J., Function of Methylated Melamine-Formaldehyde Resin in Controlling Shrinkage of Woolens, Textile Res. J. 19, 41–43 (1949).
9.
SwanepoelO. A.Van RooyenA., Machine Washing of Wool. Part 1: Type of Washing Machine, SAWTRI Tech. Rep., No. 112, (1968).
10.
Wool Science Review, “Shrink-Resist Processes for Wool: Part II. Commercial Methods,”No. 18, 18–37, 1960.