Estimation of the proportions and sulfur contents of the keratoses in thirteen, mainly South African, merino wools has shown that the plasticity of wool decreases with in creasing proportion of α-keratose and with increasing sulfur content of both α- and y-keratoses.
Get full access to this article
View all access options for this article.
References
1.
Alexander, P. and Earland, C.Textile Res. J.20, 298 (1950).
2.
Burley, R.W. , Nicholls, C.H., and Speakman. J.B., J. Textile Inst. 46, T427 (1955).
3.
Burley, R.W. and Speakman. J.B., Textile Res. J. 23, 702 (1953).
4.
Corfield, M.C. , Robson, A., and Skinner, B., Biochem. J.68, 348 (1958).
5.
Human. J.P.E. , Textile Res. J.28, 647 (1958).
6.
Jones, A.S. and Letham, D.S., The Analyst81. 15 (1955).
7.
le Roux. P. L. and Speakman, J.B., Textile Res. J.27, 1 (1957).
8.
Ripa, O. and Speakman, J.B., Textile Res. J.21, 215 (1951).
9.
Whiteley, K.J. and Speakman. J.B., Textile Res. J. 30, 46 (1960).
10.
Zahn, H. and Traumann, K., Textilber. 35. 1069 (1954).