Calculations based on apparent density measurements and X-ray diffraction data indicated that the porosity of dental stone arose from evaporation of excess water and from micropores created by crystal impingement. The volume of these created micropores was directly related to the linear expansion of the stone.
Get full access to this article
View all access options for this article.
References
1.
Worner, H.K. : Dental Plasters. I and II, Aust J Dent46:1-46, 1942.
2.
Skinner, E.W., and Phillips, R.W.: The Science of Dental Materials, 6th ed., Philadelphia, Pa.: W. B. Saunders Co.. 1967. pp 51-69.
3.
Jrgensen, K.D. : Studies on the Setting of Plaster of Paris , Odont T61:305-346, 1953.
4.
Mahler, D.B. , and Asgarzadeh, K. : The Volumetric Contraction of Dental Gypsum Materials on Setting, J Dent Res32 :354-361, 1953.
5.
Kusner, W., and Michman, J.: Setting Expansion of Plaster of Paris, J Dent Res46:661-665, 1967.
6.
Standards Association of Australia, Aust Dent Assoc Spec No T5, 1960.
7.
American Society For Testing Materials : X-ray Powder Data File, Cards 6-0046 and 6-0047, ASTM publishers , Philadelphia, Pa.
8.
Docking, A.R. ; Chong, M.D.; and Don-Nison , J.A.: The Hygroscopic Setting Expansion of Dental Casting Investments, Aust J Dent52:160-166, 1948.
9.
American Dental Association: Guide to Dental Materials. 3d ed, 1966, p 66.
10.
Cullity B.D.: Elements of X-ray Diffraction, Reading, Mass.: Addison-Wesley Publishing Co., 1956, pp 263-269.
11.
Asgar, K.; Mahler, D.B.; and Peyton, F.A.: Hygroscopic Technic for Inlay Casting upon Controlled Water Additives, J Prosth Dent5:711, 1955.