This in situ study investigated whether there is a relationship between gap size and wall lesion development in dentin next to 2 composite materials, and whether a clinically relevant threshold for the gap size could be established. For 21 days, 14 volunteers wore a modified occlusal splint containing human dentin samples with 5 different interfaces: 4 gaps of 50 µm, 100 µm, 200 µm, or 400 µm and 1 non-bonded interface without a gap. Eight times a day, the splint with samples was dipped in a 20% sucrose solution for 10 minutes. Before and after caries development, specimens were imaged with transversal wavelength-independent microradiography (T-WIM), and lesion depth (LD) and mineral loss (ML) were calculated at the 5 different interfaces. After correction for the confounder location (more mesial or distal), a paired t test clustered within volunteers was performed for comparison of gap widths. Results showed no trend for a relationship between the corrected lesion depth and the gap size. None of the differences in lesion depth for the different gap sizes was statistically significant. Also, the composite material (AP-X or Filtek Supreme) gave no statistically significant differences in lesion depth and mineral loss. A minimum gap size could not be established, although, in a non-bonded interface without a measurable gap, wall lesion development was never observed.
Keywords
Get full access to this article
View all access options for this article.
References
Supplementary Material
Please find the following supplemental material available below.
For Open Access articles published under a Creative Commons License, all supplemental material carries the same license as the article it is associated with.
For non-Open Access articles published, all supplemental material carries a non-exclusive license, and permission requests for re-use of supplemental material or any part of supplemental material shall be sent directly to the copyright owner as specified in the copyright notice associated with the article.