Composites of nickel containing 35 volume percent tungsten filaments and 11 volume percent alpha-Al 2O3 whiskers have been fabricated by the electroforming technique. Their (.2%) yield and ultimate tensile strengths after annealing (650° in H2 for 1/2 hour) have been found to be a linear function of the volume percent of the filament. The feasibility of producing nickel com posite reinforced with boron and E-glass filaments and SiC whiskers by this technique has also been demonstrated.
Get full access to this article
View all access options for this article.
References
1.
T. Vasilos and E.G. Wolff, Journal of Metals, Vol. 18, May ( 1966), p. 586.
2.
F.K. Sautter, "Electrodeposition of Dispersed-Hardened Nickel-Al2O 3 Alloys," WVT-RR-6204, February (1962).
3.
I. Ahmad, V.P. Greco and J.M. Barranco, "Electroforming of Ni Composite Reinforced with some High Strength Filaments," Watervliet Arsenal Report, under preparation.
4.
D.M. Marsh, Journal of Scientific Instruments, Vol. 36 (1959), p. 165.
5.
C.J. Smithels, Metals Reference Book, Butterworth, Washington (1962).
6.
W. Sutton, Fiber Composite Materials, ASM Symposium (1965).
7.
D.L. McDanels , R.W. Jech and J.W. Weeton, Trans. AIME , Vol. 233 (1963), p. 636.
8.
A. Kelly and W.R. Tyson, High-Strength Materials, V. L. Zackay, Edit., J. Wiley & Sons, New York, ( 1965), p. 578.
9.
J.A. Alexander , R.G. Shaver, and J.G. Withers, "A Study of Low-Denstiy, High-Strength, High-Modulus Filaments and Composites" General Technology Corp., Final Report, Contract No. NASW-1020, August (1965).
10.
R.H. Baskey , "Fiber Reinforcement of Metallic and Non-Metallic Composites," Final Report ASD-TDR 63-619, July ( 1963), p. 99.
11.
R.K. Robinson and D.L. Farnsworth, "Summary of the 10th Meeting of Refractory Composites Working Group," DMIC No. 204 (1965), p. 8.
12.
N.J. Paratt , Powder Metallurgy, Vol. 7 (1964), p. 152.