Abstract
The microstructure and corrosion properties of Ti7CuxSn (x = 0-5 wt-%) alloys after solution treatment have been investigated. The alloys were solution-treated (ST) at 1000°C for 2 h, followed by quenching in water to room temperature. It was found that the microstructure of the ST Ti7Cu alloy had only a martensite structure, and that addition of Sn could refine the microstructure of Ti7CuxSn alloy. Notably, the pseudo dendritic α-Ti phase was formed in ST Ti7Cu5Sn alloys. Potentiodynamic polarisation curves and electrochemical impedance spectroscopy data demonstrated that adding Sn improved the electrochemical corrosion behaviour of the Ti7CuxSn alloy.