A TRIP-aided bainitic-ferritic (TBF) steel with a chemical composition of Fe–0.19C–1.7Mn–1.09Si–0.51Al–0.05Nb (wt-%) was partially austenitised from a hot-rolled martensitic initial microstructure. After the hot rolling, the martensitic specimens were reheated to different intercritical temperatures and then austempered at 350°C. Thus, the effect of the initial microstructure of TBF steel on intercritical austenite formation during partial austenitisation was studied. The microstructures were investigated by scanning electron microscopy and electron backscatter diffraction (EBSD), and the tensile properties were tested. Microstructural observations revealed that a final microstructure of fine ferrite, bainitic ferrite, and retained austenite can be obtained. The steel partial austenitised at 770°C showed a good combination of ultimate tensile strength and total elongation.